> I can see no good down the path of ply construction. You still have to
glass both sides, at wet layup ratios of expensive glue. In awkward
positions and varying finishes and quality.
Im not suggesting using ply, Im suggesting using pre-made infused foam core panels, but in the fashion of ply construction or some hybrid of it.