Subject: Re:: Re: [harryproa] Re: Release wax |
From: "'.' eruttan@yahoo.com [harryproa]" <harryproa@yahoogroups.com.au> |
Date: 10/22/2018, 6:41 PM |
To: harryproa@yahoogroups.com.au |
Reply-to: harryproa@yahoogroups.com.au |
| If there is a mold involved, then this is a problem with all major processes - hand layup, vacuum bagging or infusion. With vacuum bagging and infusion the non-mold surface is covered with peel ply, then the bag, but the mold side is laid out directly on the mold with its release compound.
Sure. But I think II uses plastic as the mold release generally, as rob has said many times, because its cheap, and PP on that, then fiber. So I guess II is different.