| One solution was to weave tow through the air holes in the foam. Done a metre or so of tow at a time, it was "fairly quick" to sew a sheet. The improvement in core properties is, apparently, immense. H60 with tow performs as well as H100 under many loads. Something else to try.

I want all the details, please